| ltem | Specification |
|---|---|
| Appearance | White to pale yellow granules |
| Softening Point (Ring-and-ball method)°C | 95~110 |
| Heating loss(105°C,2h)% | ≤1.0 |
| Acid Value mg KOH/g | ≤0.1 |
| Ash content(850°C)% | ≤0.1 |
1.it has good heat resistance and good compatibility with polymer, which is help improve the glass transition temperature of the rubber, improve the vulcanized rubber 0°Ctanò and good anti-skid performance.
2.improve packing dispersion, reduce packing network effect.
3.improve adhesive compound stickiness
4.use to tyre and other rubber products.